基本磁性参数
parameters
|
纳米晶铁芯
Nanocrystalline Cores
|
铁氧体铁芯
Ferrite Cores
|
|
饱和磁感应强度Bs(T)
Saturate induction (T)
|
1.25
|
0.5
|
|
剩余磁感应强度Br(T)(20KHz)
Remanence (T) (20KHz)
|
<0.20
|
0.20
|
|
铁损 (20KHz/0.2T)(W/Kg)
Core loss(20KHz/0.2T)(W/Kg)
|
<3.4
|
7.5
|
|
铁损 (0KHz/0.5T)(W/Kg)
Core loss(0KHz/0.5T)(W/Kg)
|
<35
|
---
|
|
铁损 (50KHz/0.32T)(W/Kg)
Core loss(50KHz/0.32T)(W/Kg)
|
<40
|
---
|
|
导磁率 (20KHz)(Gs/Oe)
Permeability(20KHz)(Gs/Oe
|
>20,000
|
2,000
|
|
矫顽力 Hc (A/m)
Coercivity Hc (A/m)
|
<1.60
|
6
|
|
饱和磁致伸缩系数(×10-6)
Saturate magnetostriction×10-6
|
<2
|
4
|
|
电阻率 (mW.cm)
Resistivity (mW.cm)
|
80
|
106
|
|
居里温度 Tc (℃)
Curie temperature (℃)
|
570
|
<200
|
|
叠片系数
Stacking factor
|
>0.75
|
-
|